Optimization and Kinetic Study of Manganese Leaching from Pyrolusite Ore in Hydrochloric Acid Solutions with Oxalic Acid

MakaleAçık ErişimScopus SJRQ1
  • SDG 12 · Sorumlu Üretim ve Tüketim

Özet

The leaching behavior of pyrolusite minerals was examined in hydrochloric acid solutions, including oxalic acid, to evaluate the influence of various experimental conditions. The optimum parameters for the leaching process were found in the first stage, and the process's kinetics were assessed in the second. The concentrations of oxalic acid, hydrochloric acid, and temperature were chosen as independent variables in the optimization experiments, with the central composite design used to analyze the experimental data. The optimum concentrations for oxalic acid, hydrochloric acid, and temperature were determined to be 0.75 mol/L, 1.2 mol/L, and 60 °C, respectively. The leaching rate was determined to be 97.4% for 120 min of response time in optimum situations. The kinetic assessment experiments studied the effects of solid/liquid ratio, particle size, stirring speed, and temperature on the manganese leaching rate from pyrolusite. In the studies, the leaching rate was shown to rise with increasing temperature and stirring speed, as well as with decreasing particle size and solid/liquid ratio. The kinetic analysis revealed that the leaching kinetics matched the mixed kinetic model, and a mathematical model for the leaching process was developed. This process's activation energy was determined to be 29.05 kJ/mol. Graphical Abstract: (Figure presented.)

Anahtar Kelimeler

RDL Kalıcı Bağlantı (PID)
https://rdlopen.rawdatalibrary.net/r/munzur/1775Resmi atıflarda kullanılan kalıcı adres
DOI
https://doi.org/10.1007/s40831-024-00869-4Yayıncı resmi DOI adresi
İndeks kayıtları
Kaydın indeks veri tabanlarındaki sayfası (aktarımda alınan kayıt numarasıyla). Erişim, indeksin kendi koşullarına bağlıdır.
Atıflar
Scopus
17
WoS
15
OpenAlex
18
Her kaynağın kendi saydığı toplam atıf; aktarım ve zenginleştirme sırasında alındı.
Tam Kayıt
AlanDeğerDil
dc.contributor.authorKaracahan, Mehmet Kayra
dc.date.accessioned2026-10-28T14:54:34.084456856Z
dc.date.available2026-10-28T14:54:34.084456856Z
dc.date.issued2024
dc.description.abstractThe leaching behavior of pyrolusite minerals was examined in hydrochloric acid solutions, including oxalic acid, to evaluate the influence of various experimental conditions. The optimum parameters for the leaching process were found in the first stage, and the process's kinetics were assessed in the second. The concentrations of oxalic acid, hydrochloric acid, and temperature were chosen as independent variables in the optimization experiments, with the central composite design used to analyze the experimental data. The optimum concentrations for oxalic acid, hydrochloric acid, and temperature were determined to be 0.75 mol/L, 1.2 mol/L, and 60 °C, respectively. The leaching rate was determined to be 97.4% for 120 min of response time in optimum situations. The kinetic assessment experiments studied the effects of solid/liquid ratio, particle size, stirring speed, and temperature on the manganese leaching rate from pyrolusite. In the studies, the leaching rate was shown to rise with increasing temperature and stirring speed, as well as with decreasing particle size and solid/liquid ratio. The kinetic analysis revealed that the leaching kinetics matched the mixed kinetic model, and a mathematical model for the leaching process was developed. This process's activation energy was determined to be 29.05 kJ/mol. Graphical Abstract: (Figure presented.)
dc.description.sponsorshipTürkiye Bilimsel ve Teknolojik Araştırma Kurumu, TÜBİTAK
dc.identifier.doi10.1007/s40831-024-00869-4
dc.identifier.eissn2199-3831
dc.identifier.endpage1732
dc.identifier.issn2199-3823
dc.identifier.issue3
dc.identifier.scopus2-s2.0-85200687237
dc.identifier.startpage1717
dc.identifier.urihttps://rdlopen.rawdatalibrary.net/r/munzur/1775
dc.identifier.volume10
dc.identifier.wosWOS:001285685500002
dc.language.isoen
dc.publisherSpringer Science and Business Media Deutschland GmbH
dc.relation.ispartofJournal of Sustainable Metallurgy
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectCentral composite design
dc.subjectLeaching
dc.subjectManganese
dc.subjectOxalic acid
dc.subjectPyrolusite
dc.subject.classificationGreen & Sustainable Science & Technology
dc.subject.classificationMetallurgy & Metallurgical Engineering
dc.subject.classificationScience & Technology - Other Topics
dc.subject.otherActivation energy
dc.subject.otherHydrochloric acid
dc.subject.otherKinetic theory
dc.subject.otherKinetics
dc.subject.otherLeaching
dc.subject.otherManganese
dc.subject.otherParticle size
dc.subject.otherParticle size analysis
dc.subject.otherCentral composite designs
dc.subject.otherHydrochloric acid solution
dc.subject.otherLeaching process
dc.subject.otherLeaching rates
dc.subject.otherOptimization studies
dc.subject.otherParticles sizes
dc.subject.otherPyrolusite
dc.subject.otherSolid-liquid ratio
dc.subject.otherStirring speed
dc.subject.otherOxalic acid
dc.titleOptimization and Kinetic Study of Manganese Leaching from Pyrolusite Ore in Hydrochloric Acid Solutions with Oxalic Acid
dc.typeArticle
rdl.citation.openalex18
rdl.citation.scopus17
rdl.citation.wos15
rdl.oa.statushybrid
rdl.oa.urlhttps://doi.org/10.1007/s40831-024-00869-4
rdl.scopus.quartileQ1
rdl.sdgSDG12
rdl.source.indexSCOPUS
rdl.source.indexWOS
rdl.wos.indexScience Citation Index Expanded (SCI-EXPANDED)