Curing effect on mortar properties produced with styrene-butadiene rubber
Özet
This paper presents an experimentally investigation pertinent to the mechanical properties of rubberized mortar (RM) with styrene-butadiene rubber (SBR). The SBR were used with constant water-to-cement ratio of 0.485 and two different volume proportion of SBR particles were utilized as aggregates. One types of SBR particles with fineness modulus of 4.951 were utilized 0%, 10%, and 20% of aggregate volume. Effectiveness of SBR replacement ratio, curing and aging effect on the compressive strength, flexural strengths as well as load-displacement. Compressive and flexural strength of concrete were investigated at the end of 28-days and 56-days age. Obtained results demonstrated that utilization of SBR reduced the flexural strength of SBR mortar at the earlier curing age while SBR increased. Moreover, mechanical properties of mortar mentioned above were significantly affected by the water cure timing with an increasing proportion of the replacement level of SBR.
Anahtar Kelimeler
- Scopus
- 11
- WoS
- 11
- OpenAlex
- 13
Tam Kayıt
| Alan | Değer | Dil |
|---|---|---|
| dc.contributor.author | Cemalgil, Selim | |
| dc.contributor.author | Etli, Serkan | |
| dc.contributor.author | Onat, Onur | |
| dc.date.accessioned | 2026-10-28T14:56:31.086798994Z | |
| dc.date.available | 2026-10-28T14:56:31.086798994Z | |
| dc.date.issued | 2018 | |
| dc.description.abstract | This paper presents an experimentally investigation pertinent to the mechanical properties of rubberized mortar (RM) with styrene-butadiene rubber (SBR). The SBR were used with constant water-to-cement ratio of 0.485 and two different volume proportion of SBR particles were utilized as aggregates. One types of SBR particles with fineness modulus of 4.951 were utilized 0%, 10%, and 20% of aggregate volume. Effectiveness of SBR replacement ratio, curing and aging effect on the compressive strength, flexural strengths as well as load-displacement. Compressive and flexural strength of concrete were investigated at the end of 28-days and 56-days age. Obtained results demonstrated that utilization of SBR reduced the flexural strength of SBR mortar at the earlier curing age while SBR increased. Moreover, mechanical properties of mortar mentioned above were significantly affected by the water cure timing with an increasing proportion of the replacement level of SBR. | |
| dc.identifier.doi | 10.12989/cac.2018.21.6.705 | |
| dc.identifier.eissn | 1598-818X | |
| dc.identifier.endpage | 715 | |
| dc.identifier.issn | 1598-8198 | |
| dc.identifier.issue | 6 | |
| dc.identifier.scopus | 2-s2.0-85049694236 | |
| dc.identifier.startpage | 705 | |
| dc.identifier.uri | https://rdlopen.rawdatalibrary.net/r/munzur/3343 | |
| dc.identifier.volume | 21 | |
| dc.identifier.wos | WOS:000435651700009 | |
| dc.language.iso | en | |
| dc.publisher | Techno Press | |
| dc.relation.ispartof | Computers and Concrete | |
| dc.rights | info:eu-repo/semantics/closedAccess | |
| dc.subject | Fineness modulus | |
| dc.subject | Mechanical properties | |
| dc.subject | Rubberized mortar | |
| dc.subject | Styrene-butadiene rubber | |
| dc.subject.classification | Computer Science, Interdisciplinary Applications | |
| dc.subject.classification | Construction & Building Technology | |
| dc.subject.classification | Engineering, Civil | |
| dc.subject.classification | Materials Science, Characterization & Testing | |
| dc.subject.classification | Computer Science | |
| dc.subject.classification | Engineering | |
| dc.subject.classification | Materials Science | |
| dc.subject.other | Aggregates | |
| dc.subject.other | Bending strength | |
| dc.subject.other | Butadiene | |
| dc.subject.other | Curing | |
| dc.subject.other | Mechanical properties | |
| dc.subject.other | Mortar | |
| dc.subject.other | Rubber | |
| dc.subject.other | Styrene | |
| dc.subject.other | Compressive and flexural strengths | |
| dc.subject.other | Fineness modulus | |
| dc.subject.other | Load displacements | |
| dc.subject.other | Mortar properties | |
| dc.subject.other | Replacement level | |
| dc.subject.other | Replacement ratio | |
| dc.subject.other | Styrene butadiene rubber | |
| dc.subject.other | Water to cement (binder) ratios | |
| dc.subject.other | Compressive strength | |
| dc.title | Curing effect on mortar properties produced with styrene-butadiene rubber | |
| dc.type | Article | |
| rdl.citation.openalex | 13 | |
| rdl.citation.scopus | 11 | |
| rdl.citation.wos | 11 | |
| rdl.oa.status | closed | |
| rdl.scopus.quartile | Q2 | |
| rdl.source.index | SCOPUS | |
| rdl.source.index | WOS | |
| rdl.wos.index | Science Citation Index Expanded (SCI-EXPANDED) |