Özet

Recently, various types of additives are being used to enhance the properties of bitumen. Until now, few researchers have handled the utilization of different additives in the same binder. In this study, styrene-butadiene-styrene (SBS) and Evotherm were used both separately and in the same blend. Dynamic shear rheometer (DSR) and bending beam rheometer (BBR) tests were applied to SBS and Evotherm modified binders. SBS and Evotherm were added to pure bitumen in three different ratios. Sixteen different combinations were produced using the two additives, and a pure binder in the same binder was evaluated in the DSR test. Eight different combinations were evaluated in the BBR test. The conclusion reached was that the maximum usage of Evotherm (0.9%) induces a 20% reduction in the rutting parameter of both the 5% and 6% SBS modified binders. The 0.5% Evotherm with 4% and 5% SBS modification does not have an adverse effect on rutting performance. Evotherm modification could prevent the stiffness increment that originates from using the SBS additive, especially at high content. Using 0.7% Evotherm with 4% SBS can acquire the pure binder's low temperature performance. (c) 2019 American Society of Civil Engineers.

Anahtar Kelimeler

RDL Kalıcı Bağlantı (PID)
https://rdlopen.rawdatalibrary.net/r/munzur/4708Resmi atıflarda kullanılan kalıcı adres
İndeks kayıtları
Kaydın indeks veri tabanlarındaki sayfası (aktarımda alınan kayıt numarasıyla). Erişim, indeksin kendi koşullarına bağlıdır.
Atıflar
WoS
11
Her kaynağın kendi saydığı toplam atıf; aktarım ve zenginleştirme sırasında alındı.
Tam Kayıt
AlanDeğerDil
dc.contributor.authorKök, Baha Vural
dc.contributor.authorYilmaz, Mehmet
dc.contributor.authorAkpolat, Mustafa
dc.date.accessioned2026-10-28T15:03:38.984590260Z
dc.date.available2026-10-28T15:03:38.984590260Z
dc.date.issued2019-04
dc.description.abstractRecently, various types of additives are being used to enhance the properties of bitumen. Until now, few researchers have handled the utilization of different additives in the same binder. In this study, styrene-butadiene-styrene (SBS) and Evotherm were used both separately and in the same blend. Dynamic shear rheometer (DSR) and bending beam rheometer (BBR) tests were applied to SBS and Evotherm modified binders. SBS and Evotherm were added to pure bitumen in three different ratios. Sixteen different combinations were produced using the two additives, and a pure binder in the same binder was evaluated in the DSR test. Eight different combinations were evaluated in the BBR test. The conclusion reached was that the maximum usage of Evotherm (0.9%) induces a 20% reduction in the rutting parameter of both the 5% and 6% SBS modified binders. The 0.5% Evotherm with 4% and 5% SBS modification does not have an adverse effect on rutting performance. Evotherm modification could prevent the stiffness increment that originates from using the SBS additive, especially at high content. Using 0.7% Evotherm with 4% SBS can acquire the pure binder's low temperature performance. (c) 2019 American Society of Civil Engineers.
dc.identifier.articlenumber4019023
dc.identifier.doi10.1061/(asce)mt.1943-5533.0002654
dc.identifier.eissn1943-5533
dc.identifier.issn0899-1561
dc.identifier.issue4
dc.identifier.urihttps://rdlopen.rawdatalibrary.net/r/munzur/4708
dc.identifier.volume31
dc.identifier.wosWOS:000482217400019
dc.language.isoen
dc.publisherASCE-AMER SOC CIVIL ENGINEERS
dc.relation.ispartofJOURNAL OF MATERIALS IN CIVIL ENGINEERING
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectStyrene-butadiene-styrene
dc.subjectEvotherm
dc.subjectRutting parameter
dc.subjectLow temperature resistance
dc.subject.classificationConstruction & Building Technology
dc.subject.classificationEngineering, Civil
dc.subject.classificationMaterials Science, Multidisciplinary
dc.subject.classificationEngineering
dc.subject.classificationMaterials Science
dc.subject.otherWARM MIX ASPHALT
dc.subject.otherSTYRENE-BUTADIENE-STYRENE
dc.subject.otherRHEOLOGICAL PROPERTIES
dc.subject.otherGRADE
dc.titlePerformance Evaluation of Using Evotherm in SBS Modified Binder
dc.typeArticle
rdl.citation.wos11
rdl.oa.statuspreprint
rdl.oa.statusgreen
rdl.oa.urlhttps://hdl.handle.net/11508/57225
rdl.scopus.quartileQ1
rdl.source.indexWOS
rdl.wos.indexScience Citation Index Expanded (SCI-EXPANDED)